Sample Info
- sample_name
- Stingray
- sample_id
- details
E6 CVD
50 μm thin sample
EL SC
polished
14N 60-keV implant, 10° tilt (InnovION)
[N] = 1 x 109 cm-2
- Photo
- side 1
- side 2
- strain
- image_other1
- imager_other2
- location
- CNS Toolbox
- user
- Huiliang
- date
- user log
- impl.
- 14N
- dose (cm^-2)
- energy (keV)
- 13C (%)
- N (cm^-3)
- N (ppm)
- NV (cm^-3)
- NV- (ppm)
- annealing temp. (C)
- annealing time (hours)
- annealing_history
- irradiation
- beam flux (1/cm^2 1/s)
- irradiation_time (hours)
- irradiation_history
- grower
- E6
- type
- CVD Chip
- layer thknss (μm)
- growth date
- dimen.
- surface
- edge
- C (%)
- T2* (μs)
- max t2star
- T2 (μs)
- max t2
- T1 (ms)
- substr.