Sample Info
- sample_name
- Storm-B
- sample_id
- E13c-10-1-B
- details
E6 CVD
10% 13C enriched layer1.1% 13C
ELSC substrate
polished
14N 85-keV implant, 0° tilt
[N] = 2 x 1012 cm-2
- Photo
- side 1
- side 2
- strain
- image_other1
- imager_other2
- location
- ImagerOne Desk
- user
- Erik
- date
- 04/16
- user log
Erik – April 2016
Characterization in Imager One confocal see here, this sample was supposed to be 10% 13C, but only seems to have 1.1%
- impl.
- N14
- dose (cm^-2)
- 2E12
- energy (keV)
- 85
- 13C (%)
- N (cm^-3)
- N (ppm)
- NV (cm^-3)
- NV- (ppm)
- annealing temp. (C)
- annealing time (hours)
- annealing_history
- irradiation
- beam flux (1/cm^2 1/s)
- irradiation_time (hours)
- irradiation_history
- grower
- E6
- type
- 1
- layer thknss (μm)
- growth date
- dimen.
- surface
- edge
- 1
- C (%)
- 2.5
- T2* (μs)
- 0.75
- max t2star
- 0.75
- T2 (μs)
- 120 – 140
- max t2
- 131
- T1 (ms)
- 5.1
- substr.